(620) 488-2282 orders@kansascastings.com Majority woman-owned Made in USA
Materials guide

Gray, Ductile & White Iron: Which Cast Iron Do You Need?

“Cast iron” isn’t one material — it’s a family, and the three we pour behave very differently. The short version: gray iron for rigid, vibration-damping parts, ductile iron for load-bearing strength, and high-chrome white iron — our specialty — when a part is wearing out from abrasion. Here’s how to tell them apart and spec the right one.

The 30-second answer

It comes down to how the graphite sits

Every cast iron is iron plus carbon — what changes is the shape the carbon takes. In gray iron it’s graphite flakes (easy to machine, great at damping, brittle in tension). In ductile iron it’s graphite spheres (real strength and give). In white iron the carbon is locked up as hard iron carbide instead of free graphite — which is what makes it so brutally hard and wear-resistant. Get the carbon shape right for your load and the part lasts; get it wrong and it washes out or cracks.

Side by side

The three irons we pour, compared on the properties that actually drive the decision.

 Gray ironDuctile ironWhite iron ★
StandardASTM A48ASTM A536ASTM A532 (high-chrome)
Carbon formGraphite flakesGraphite spheres (nodular)Iron carbide — no free graphite
Typical hardness150–260 HB150–300 HB450–700+ HB (to ~800 hardened)
Tensile strengthLow (strong in compression)High (60–100k+ psi)Low — hard but brittle
Ductility / impactBrittleDuctile, takes impactBrittle by design
Wear resistanceModerateModerateExceptional
Best atRigidity, damping, machinabilityLoad-bearing strengthAbrasion & surface wear

★ High-chrome white iron is our specialty. Values are standard ASTM reference ranges — see the full materials & specs.

Gray iron · ASTM A48

When you want rigidity and quiet

Those graphite flakes are little stress risers, so gray iron is brittle in tension — but they also make it the easiest iron to machine, excellent at damping vibration and noise, and very strong in compression. It’s the classic choice for machine bases, housings, manifolds, pulleys, and counterweights — parts that need to sit still, stay rigid, and soak up vibration rather than carry a bending load. See gray iron →

Ductile iron · ASTM A536

When the part has to carry a load

Round off the graphite into spheres and the iron stops being brittle: ductile iron (also called nodular iron) pulls real tensile strength and elongation out of the same base metal, so it bends before it breaks. That makes it the pick for brackets, hubs, gears, housings under pressure, and any part that takes structural or shock load where gray iron would fracture. See ductile iron →

White iron · ASTM A532 · our specialty

When the enemy is abrasion

When a part isn’t breaking but wearing out — grinding, sliding, eroding against hard media — neither gray nor ductile iron will last. High-chrome white iron will. With its carbon locked up as hard chromium carbide, it runs 450 to 700+ Brinell (up to ~800 HB heat-treated) and outlasts ordinary iron many times over in crusher liners, slurry-pump volutes and impellers, tillage wear parts, and chute liners. It’s intentionally hard and brittle, so it’s chosen for surface wear rather than structural load — and it’s the iron we pour best. See white iron →

How to choose, fast

Start with how the part fails — or is expected to fail — in service.

It’s wearing out → White iron

Abrasion, erosion, sliding against hard media. You’re replacing it too often. High-chrome white iron, ASTM A532.

It’s cracking under load → Ductile iron

Structural, bending, or impact load. You need strength and give. Ductile iron, ASTM A536.

It needs to stay rigid & quiet → Gray iron

Machine bases, housings, damping, compression. Easy to machine. Gray iron, ASTM A48.

Not sure? → Send it to us

Give us the drawing or a worn sample and how it fails. We’ll recommend the grade and quote it — no minimum.

Frequently asked

Cast iron, answered

What is the difference between gray iron and ductile iron?
Gray iron has graphite in flakes, which makes it easy to machine, good at damping vibration, and strong in compression — but brittle in tension. Ductile iron has graphite in spheres (nodules), which gives it real tensile strength and ductility, so it bends before it breaks. Choose gray for rigid, vibration-damping parts; choose ductile for load-bearing parts that must not fracture.
Which cast iron is the hardest?
High-chrome white iron, by far — typically 450 to 700+ Brinell, and up to about 800 HB heat-treated. Gray and ductile iron are much softer because their graphite is free rather than locked up as iron carbide. White iron is the choice whenever abrasion and wear life are the priority.
Which cast iron is strongest?
For tensile strength and impact, ductile iron — common grades run 60,000 to 100,000+ psi tensile with meaningful elongation. Gray iron is strong in compression but weak in tension. White iron is hard but brittle, so it isn't used for structural strength. Match the iron to the load: ductile for pulling and bending, gray for rigid compression, white for surface wear.
When should I use white iron instead of gray or ductile iron?
Use high-chrome white iron (ASTM A532) when a part is wearing out from abrasion — crusher liners, slurry-pump components, tillage wear parts, chute liners. It outlasts gray and ductile iron many times over in sliding, abrasive service, and it's our specialty. Use gray or ductile iron when the part carries structural or impact load rather than surface wear.
Can Kansas Castings help me choose the right iron?
Yes. Send a drawing or a worn sample with how it fails in service and we'll recommend the grade — gray, ductile, or high-chrome white iron — and quote it. We pour parts up to 150 lb with no minimum, cast in Belle Plaine, Kansas since 1993, with material certs on request.
Request a quote

Not sure which iron your part needs?

Send your drawing or a worn sample and tell us how it fails — we’ll recommend gray, ductile, or high-chrome white iron and quote it. Up to 150 lb, no minimum.