(620) 488-2282 orders@kansascastings.com Majority woman-owned Made in USA
Wear-iron guide · ASTM A532

Ni-Hard vs. High-Chrome White Iron: Which Wears Longer?

Both are white irons — both are ASTM A532 — and both are poured for one job: surviving abrasion. The difference is how they survive it. Ni-Hard (Class I) trades a little hardness for a tougher matrix that shrugs off impact. High-chrome (Class II/III) — our specialty — forms harder carbides and wears longer in pure sliding and erosive service. Here’s how to pick.

The 30-second answer

Same standard, different carbide

Ni-Hard and high-chrome are both ASTM A532 white irons, so both lock their carbon up as hard carbide instead of free graphite. What sets them apart is the carbide. Ni-Hard’s nickel-chromium chemistry forms a continuous network of M3C iron carbide — hard, but interconnected. High-chrome forms discrete, harder M7C3 chromium carbides sitting in a tougher matrix. Those harder, less-connected carbides are why high-chrome resists fine sliding and erosive wear better — while Ni-Hard’s more forgiving structure takes impact without cracking. Match the carbide to how the part actually fails and it lasts.

Side by side

The two A532 wear irons we pour, compared on what actually drives the decision.

 Ni-HardHigh-chrome ★
ASTM A532 classClass I (Ni-Cr)Class II & III
AlloyNickel-chromium, ~3–5% NiHigh chromium, ~20–28% Cr (+Mo)
Carbide typeM3C iron carbide (continuous network)M7C3 chromium carbide (discrete, harder)
Typical hardness550–650 HB600–750 HB (to ~800 hardened)
Impact toleranceBetter — tougher matrixLower — harder but more brittle
Sliding / erosive abrasionGoodExceptional
Corrosion & hot wearLimitedBetter — chromium helps
Heat-treat responseLimitedStrong — destabilize & harden
Best atImpact + abrasion togetherMaximum sliding & erosive wear

★ High-chrome white iron is our specialty. Values are standard ASTM A532 reference ranges — see the full materials & specs.

Ni-Hard · A532 Class I

When impact rides along with the wear

Ni-Hard’s nickel-chromium chemistry gives it a martensitic matrix that’s tougher than high-chrome’s — so it tolerates repeated impact while still holding 550–650 Brinell. That makes it a long-running choice for grinding-mill liners, pump casings, and parts that take blows as well as abrasion. It’s a proven, decades-old wear grade, and where the duty is gouging or impact-plus-abrasion rather than pure sliding, it’s often the right call.

High-chrome · A532 Class II/III · our specialty

When it’s pure abrasion, and you want the most life

Push the chromium up to 20–28% and the iron forms hard M7C3 chromium carbides that resist fine, sliding, and erosive abrasion far better than Ni-Hard’s iron carbide. High-chrome runs 600–750 HB as-cast and can be heat-treated toward ~800 HB, holds hardness at elevated temperature, and brings some corrosion resistance along with it. For crusher liners, slurry-pump volutes and impellers, chute liners, and tillage wear parts, it’s the grade that wears longest — and the one we pour best. See white iron →

How to choose, fast

Start with what’s actually killing the part.

Pure sliding / erosion → High-chrome

Slurry, fine abrasives, chute and liner wear with little impact. Maximum life. A532 Class II/III.

Impact + abrasion → Ni-Hard

Grinding-mill liners, pump casings, parts taking blows as well as wear. Tougher matrix. A532 Class I.

Heat or mild corrosion → High-chrome

Holds hardness hot and resists some corrosion the chromium brings. A532 Class II/III.

Not sure? → Send it to us

Give us the drawing or a worn sample and how it fails. We’ll recommend the A532 grade and quote it — no minimum.

Frequently asked

Ni-Hard vs. high-chrome, answered

Is Ni-Hard the same as white iron?
Yes. Ni-Hard is a white iron — it's ASTM A532 Class I, a nickel-chromium (Ni-Cr) grade. High-chrome white iron is the same standard's Class II and III. Both lock their carbon up as hard carbide instead of free graphite; they differ in alloy and carbide type, not in being white iron.
Which is harder, Ni-Hard or high-chrome white iron?
High-chrome is generally harder and more abrasion-resistant. Ni-Hard runs about 550–650 Brinell; high-chrome runs about 600–750 Brinell and can be heat-treated toward 800 HB. High-chrome also forms harder M₇C₃ chromium carbides versus Ni-Hard's M₃C iron carbides, which is why it lasts longer in sliding and erosive wear.
When is Ni-Hard the better choice?
Where impact comes with the abrasion — grinding-mill liners, pump casings, and parts that take repeated blows as well as wear. Its tougher matrix tolerates impact better than high-chrome. For pure sliding or erosive abrasion with little impact, high-chrome wears longer.
Can high-chrome white iron be heat-treated?
Yes. High-chrome grades are commonly destabilized and hardened to raise hardness and wear life, reaching up to about 800 HB. Ni-Hard's hardening response is more limited. If you need the most wear life from heat treatment, high-chrome is the grade to spec.
Which white iron should I order from Kansas Castings?
Tell us how the part fails. For maximum sliding, erosive, or slurry abrasion we usually recommend high-chrome white iron — it's our specialty. Where the part also takes impact, Ni-Hard may fit better. Send a drawing or a worn sample and we'll recommend the ASTM A532 grade and quote it, up to 150 lb with no minimum. New to the grades? Start with our guide to choosing gray, ductile, or white iron.
Request a quote

Spec’ing a wear part in white iron?

Send your drawing or a worn sample and how it fails — we’ll recommend Ni-Hard or high-chrome and quote it. Up to 150 lb, no minimum.